PRODUCT | PRODUCT CODE |
Paraffinated Clear | 37 |
Transperent Base Coat | 37 A |
White Base Coat | 38 |
Pigmented White | 38 A |
Pigmented Black | 38 B |
Catalyst | 49 |
Accelerator | 50 |
Catalyst - Extra Clear | 51 |
PRODUCT DESCRIPTION
WOODPOL POLYESTER LAMINATION is a three component, air-drying Polyester based wood finishing system consisting of Base Resin, Accelerator & Catalyst. It gives a clear smooth finish with a hard mirror like gloss that protects and preserve natural beauty of wood.
The excellent features of this product are:
• Easy to apply
• Quick Drying
• Very good adhesion
• Excellent filling properties
• Easy to stand
• Very high gloss
• Very high build capabilities.
• Limited yellowing.
• High surface hardness & heat resistance
• Excellent chemical, solvent & stain resistance
And hence highly recommended for finishing of table top, bedroom furniture, internal doors, kitchen bench top, etc.
APPLICATIONS PROCEDURE
» Wood article to be coated must be dry and free of dust & loose particles. Sand the surface along grains with emery paper #180. Apply stains at this stage if necessary.
» Apply one coat of WOODPOL Epoxy Primer Base coat 1:1 Base & Hardner & allow it dry for 45 to 180 minutes, apply Polyester Lamination in period 45 to 180 minutes only.
1 | Product Description | Three Component Unsaturated Polyester clear finish. |
2 | Recommended Use | Interior wood application. |
3 | Mixing ratio by wt. | Base – 100 Accelerator 2% Catalyst – 2% |
4 | Application Viscosity | Ready to use. |
5 | Pot-life of mixture | 7 – 8 minutes @ 30 °C |
6 | Shelf-life | 3 month in unopened condition when store in cool and dry place @ 25+/_5 °C. |
7 | Packing | 1kg, 4 kgs, 20 kgs |
» Mix WOODPOL POLYESTER LAMINATION with 2% of Accelerator first, mix well. Then add 2% of Catalyst, mix well. Prepare only spray gun cup capacity mixture maximum, as Pot-life of mixture is short.
» Once mixed with Catalyst, pot-life of mixture is 7-8 minutes only. First apply one cross coat & let it dry up to touchdry than apply at least 5-6 coats depending upon build require.
» Allow it to dry for minimum of 24 hours. Sand with 150 to 600 grit paper (dry sanding) followed by water cutting with 600 to 1200 grit paper.
» Carry out buffing with good quality Buffing Compound/ paste to hard mirror like glass
Warning:
Never Pre mix Accelerator and Catalyst as explosion may be the result.